The following procedure was established; About gram of the fusion flux were use to fused gram of a finely ground iron ore. The lithium borate flux and sample was place in such a way that a few millimeter of the crucible bottom was covered with lithium flux before the sample was then placed on it with the remaining fusion flux.
ANALYSIS OF IRON ORE USING XRF